![]() Tempering Hardness : HB240-280 Nitrided Hardness : HV850-1000° Nitrided Depth : 0.45-0.7mm Nitrided Brittleness : Less than or equal to 2 stages Surface Roughness : Ra 0.4 Screw Straightness : 0.015mm Chromium-plating Surface Hardness after Nitriding : More than or equal to 900HV Chromium-plating Depth : 0.05-0.10mm Dual Alloy Hardness : HRC55-60° Dual Alloy Depth : 2.0-3.0mm In order to meet customer's demand, we provide various designs such as Wave Type, Barrier Type, Mutant Type, Gradual-Change Type, Shunt Type, Exhausted type, and Separated Type, Mixed Type, Pin Type, Double Scree Type, and Multi Head Type |
|||||
Materials : 38 CrMoALA(JIS SACM645), 42 CrMo(JIS SCM440), 9 Cr18MoV, CW6M05Cr4V2, and 9Cr18MoV Alloy and Steel of High Quality (Iron, Tungsten, Nickel, Molybdenum, Duplex Stainless Steel, and Powder Metallurgy Material) Advanced Nitriding Technology Spraying Technology of corrosion and wear resisting thermometal Cold and Hot spraying technology of hard metal ![]() |
|||||
![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() |
|||||